Nickel superalloy pipe fitting cap

Nickel
superalloy pipe fitting cap

分类:

ype

Butt welded  Pipe Cap

Size

SMLS Elbow 1/2″~24″ (DN15 – DN600)

Welded Elbow 1/2″~48″ (DN15 – DN1200)

Wall thickness

sch10, sch20, sch30, std, sch40, sch60,

xs, sch80, sch100, etc

Standards

ASME, ASTM, DIN, JIS, etc

Material

Carbon Steel: ASTM: SA105N/A105, ASTM SA350 LF2,etc

Stainless Steel: ASTM A182 F304/304L/316/316L, etc

Alloy Steel: ASTM A182 F1/F5/F9/F11/F22/F91, Etc.

Duplex stainless steel: ASTM A182 F51/F53/F55/F60, etc

Nicke alloys: Nickel 200, Monel 400, Inconel 600/625, Incoloy 825/800, 

Hastelloy C276, Hastelloy C22, Hastelloy B1/B2/B3, Alloy 20, etc

Cu-Ni: 90/10,70/30, etc

Surface treatment

Transparent oil, rust-proof black oil or hot galvanized

Applications

Petroleum, chemical, power, gas, metallurgy, shipbuilding, construction, etc

Dimensions Butt Weld Caps NPS 1/2 – 48 ASME B16.9

CAP ASME B.16.9
NPS O.D.
D
LENGTH
H
LENGTH
H1
1/2 21.3 25 25
3/4 26.7 25 25
1 33.4 38 38
1.1/4 42.2 38 38
1.1/2 48.3 38 38
2 60.3 38 44
2.1/2 73 38 51
3 88.9 51 64
3.1/2 101.6 64 76
4 114.3 64 76
5 141.3 76 89
6 168.3 89 102
8 219.1 102 127
10 273 127 152
12 323.8 152 178
14 355.6 165 191
16 406.4 178 203
CAP ASME B.16.9
NPS O.D.
D
LENGTH
H
LENGTH
H1
18 457 203 229
20 508 229 254
22 559 254 254
24 610 267 305
26 660 267
28 711 267
30 762 267
32 813 267
34 864 237
36 914 267
38 965 305
40 1016 305
42 1067 305
44 1118 343
46 1168 343
48 1219 343
General notes..
  • Dimensions are in millimeters unless otherwise indicated.
  • Wall thickness (t) must be specified by customer.
  • The shape shall be ellipsoidal and shall conform to the requirements given in the ASME Boiler and Pressure Vessel Code.
  • Length (H) applies for thickness not exceeding that given in column “Wall Thickness” for Length, H.
  • Length (H1) applies for thickness greater than that given in column “Wall Thickness” for NPS 24 and smaller. For NPS 26 and larger, length H1 shall be by agreement between the manufacturerand purchaser.

Dimensional Tolerances of End Caps ASME B16.9

Nominal Pipe Size 1/2 to 2.1/2 3 to 3.1/2 4 5 to 8
Outside Diameter
at Bevel (D)
+ 1.6
– 0.8
1.6 1.6 + 2.4
– 1.6
Inside Diameter at End 0.8 1.6 1.6 1.6
Overall Length (H) 3 3 3 6
Nominal Pipe Size 10 to 18 20 to 24 26 to 30 32 to 48
Outside Diameter
at Bevel (D)
+ 4
– 3.2
+ 6.4
– 4.8
+ 6.4
– 4.8
+ 6.4
– 4.8
Inside Diameter at End 3.2 4.8 + 6.4
– 4.8
+ 6.4
– 4.8
Overall Length (H) 6 6 10 10
Wall Thickness (t) Not less than 87.5% of Nominal Wall Thickness

Dimensional tolerances are in millimeters unless otherwise indicated and are equal ± except as noted.

Note..
MSS SP-43 only covers stainless steel buttweld fittings made for use with Schedule 5S and 10S pipe and Stub Ends suitable for use with Schedule 40S pipe, as defined in ASME B36.19. The dimensions and dimensional tolerances defined in MSS SP-43 are substantially the same as those in ASME B16.9 specifications from NPS 1/2 – NPS 24. Except with regard to the outside diameter at the bevel.

dots

Weights of Buttweld Caps

SCHEDULE STD XS 160 XXS

Weights, Dimensions of Butt Weld End Caps
NPS STD XS SCH 160 XXS
1 0.09 0.14 0.18 0.23
1.1/4 0.14 0.18 0.23 0.34
1.1/2 0.18 0.23 0.27 0.41
2 0.27 0.34 0.57 0.68
2.1/2 0.41 0.45 0.79 1.13
3 0.68 0.79 1.32 1.81
3.1/2 0.91 1.13 2.72
4 1.13 1.36 2.68 3.4
5 2.04 2.49 4.54 5.44
6 2.95 4.08 6.8 8.16
8 5.44 7.26 14.06 13.61
10 9.07 11.34 25.85
12 13.61 16.33 43.09
14 16.33 20.41
16 18.14 24.49
18 24.49 32.66
20 34.02 39.01
22 42.64 56.7
24 43.54 58.97
26 53.98 72.12
30 78.02 103.87
NPS STD XS SCH 160 XXS

Note..

  • All weights are in pounds and kilograms and approximated or estimated.

Buttweld Fitting Weights

ASME buttweld fitting specifications do not specify weights for fittings. Weights quoted in the table on this page are based on manufacturers information and should be considered as approximate and provided as a guide only (fitting weights can vary considerably between manufacturers due to differences in construction).

评价

目前还没有评价

成为第一个“Nickel superalloy pipe fitting cap” 的评价者

您的邮箱地址不会被公开。 必填项已用 * 标注